Super Invar Alloy Physical Properties |
||
|---|---|---|
| Density | lb/cu in |
0.294 |
| Specific Gravity | 8.15 |
|
| Curie Temp | °F |
535 |
°C |
279 |
|
| Melting Point | °F |
2600 |
°C |
1454 |
|
| Electrical Resistivity | Micro-ohm-cm |
80 |
Micro-ohm-cm |
481.3 |
|
| Thermal Conductivity | W/cm °C |
---- |
BTU-in/sq. ft-hr- |
---- |
|
| Specific Heat | Cal/g- °C |
---- |
BTU/lbm- °F |
---- |
|
| Thermal Expansion | ppm/°F (75°F to 842°F) |
---- |
ppm/°C (25°C to 450°F) |
---- |
|
Super Invar Alloy Mechanical Properties |
||
|---|---|---|
| Tensile Strength | ksi |
70 |
MPa |
483 |
|
| Yield Strength | ksi |
40 |
MPa |
276 |
|
| Elongation | %
in 2 in. |
40 |
| Typical Hardness Ann. | Rockwell |
HRB
75 |
| Modulus of Elasticity | Mpsi |
21
x 103 |
kMPa |
---- |
|
Super Invar Alloy Chemistry |
|
|---|---|
| maximum % unless noted | |
| Iron | Bal |
| Nominal Nickel | 32 |
| Nominal Cobalt | 5 |
| Carbon | 0.02 |
| Silicon | 0.25 |
| Maganese | 0.04 |